C-67600
Chemical Composition
(%max, unless shown as range or min)
Cu* |
Fe |
Mn |
Sn |
Zn |
Pb |
|
Min/Max |
57.0-60.0 |
0.40-1.3 |
0.05-0.50 |
0.50-1.5 |
Rem |
0.50-1.0 |
Note: Cu + Sum of Named Elements, 99.5% min.
Applicable Specifications
* Bar, Rod – ASTM B138
* QQB-728
Fabrication Properties
Joining Technique | Suitability |
Soldering | Excellent |
Brazing | Excellent |
Oxyacetylene Welding | Good |
Gas Shielded Arc Welding | Fair |
Coated Metal Arc Welding | Fair |
Spot Weld | Good |
Seam Weld | Good |
Butt Weld | Good |
Capacity for Being Cold Worked | Poor |
Capacity for Being Hot Formed | Excellent |
Forgeability Rating | 80 |
Machinability Rating | 60 |
Mechanical Properties (ASTM B150)
US Customary | Metric | |
Melting Point – Liquidus | 1630 F | 890C |
Melting Point – Solidus | 1590F | 865C |
Density | 0.302 lb/in3 at 68 F | 8.36 gm/cm3 at 20 C |
Specific Gravity | 8.36 | 8.36 |
Electrical Resistivity | 116 ohms-cmil/ft at 68 F | 19.28 microhm-cm at 20 C |
Electrical Conductivity | 24 %IACS at 68 F | 0.139 MegaSiemens/cm at 20 C |
Thermal Conductivity | 61 Btu · ft/(hr · ft2·°F) at 68 F | 105.7 W/m ·°K at 20 C |
Coefficient of Thermal Expansion | 9·10-6 per °F (68-572 F) | 16.2·10-6 per °C (20-300 C) |
Specific Heat Capacity | 0.09 Btu/lb/°F at 68 F | 377.1 J/kg · °K at 20 C |
Modulus of Elasticity in Tension | 15000ksi | 103400MPa |
Modulus of Rigidity | 5600 ksi | 38600MPa |